Cleaning Trial Summary

:: TSR #15-A-237

 

Customer Objective

The customer was looking to improve their cleaning performance, automate their cleaning process and clean mixed metals together.

Cleaning Trial Type
Temperature
Aqueous
Temperature
150°F
Industry
Time Required
Industry
Metal parts manufacturing
Time Required
15 minutes to 1 hour
Segment
Substrate
Fabricated Metal Product
Steel
Soil
, Cutting Fluids
Description of Part(s)
Description of Part
Coupons
Cleaner Used
Machine Used
Machine Used

1.       Spray Under Immersion Washer (Graymills T12, Graymills T24, SK 81.8 w/SUI)

2.       Spray Washer (JRI TL3, JRI FL250, JRI FL500, Better Engineering G-2000)

Post Cleaning
Post Cleaning

Fresh water rinse followed by air pressure drying.

Recommendation to Customer
Recommendation

The ArmaKleen Technical Center recommended using 5% by volume ArmaKleen™ 4 in 1 Cleaner at 150°F in either a Spray Under Immersion Washer or a Spray Washer for a minimum of 15 minutes to 1 hour.