Skip to main content
Before
After

Cleaning Trial Summary

Segment
:: TSR #13-A-039

 

Customer Objective

The customer was looking to improve their cleaning process, automate their cleaning process, reduce rework and reject rate and recover scrap parts.

Cleaning Trial Type
Temperature
Aqueous
Temperature
160⁰F
Industry
Time Required
Industry
Copier remanufacturing
Time Required
2 hours
Segment
Substrate
Retail Trade
Aluminum Plastic Stainless Steel Steel
Soil
Grease Grime Oil Rust/Oxides Shop Dirt, Toner Residue
Description of Part(s)
Description of Part
Copier machine parts
Cleaner Used
Machine Used
Machine Used
  1. Spray Under Immersion Washer (T12, T24, 40.1, 81.8 w/ SUI)
  2. Agitating Immersion Washer (81.8, T12, T24)
  3. Spray Washer (TL3, FL250, FL500)
Post Cleaning
Post Cleaning

Fresh water rinse followed by air pressure drying.

Recommendation to Customer
Recommendation

The ArmaKleen Technical Center recommended using 5% by volume ArmaKleen™ 4 in 1 Cleaner at 160⁰F in a Spray Under Immersion Washer, an Agitating Immersion Washer or a Spray Washer for a minimum of 2 hours.