Cleaning Trial Summary
Customer Objective
Improve cleaning performance and automate cleaning process
Cleaning Trial Type
Temperature
Polymer
Temperature
160°F
Industry
Time Required
Industry
Engineered Products Manufacturing
Time Required
8-14 hours
Segment
Substrate
Non-metal Manufacturing
Iron
Steel
Soil
Thermoplastic Elastomer, Thermoplastic Valcanigales
Description of Part(s)
Description of Part
Extrusion components
Cleaner Used
10% by volume ARMAKLEEN™ M-301
100% by volume ARMAKLEEN™ Paint & Ink Remover
Machine Used
Machine Used
Ultrasonic Washer (SK Blackstone 6315)
Post Cleaning
Post Cleaning
Fresh water rinse and air pressure dried
Recommendation to Customer
Recommendation
The ArmaKleen Technical Center recommends using a 100% by volume of ArmaKleen™ Paint & Ink Remover at 160°F in an Ultrasonic Washer for a minimum of 8 to 14 hours