Skip to main content
Before
After

Cleaning Trial Summary

 

Customer Objective

Improve cleaning performance, automate cleaning process, reduce rework and reject rate, reduce need for manual cleaning

Cleaning Trial Type
Temperature
Adhesive
Temperature
160°F
Industry
Time Required
Industry
Aerospace
Time Required
30 minutes
Segment
Substrate
Transportation Equipment Manufacturing
Aluminum
Soil
Adhesive (3M 27), Fiber Board (Meduium Density)
Description of Part(s)
Description of Part
Oblong disks
Cleaner Used

10% by volume ARMAKLEEN™ M-Aero

Machine Used
Machine Used

Agitating Immersion Washer (SK Model 81.8, Graymills T12, Graymills T24)

Post Cleaning
Post Cleaning

Fresh water rinse and air pressure drying

Recommendation to Customer
Recommendation

The ArmaKleen Technical Center recommends using a 10% by volume solution of ArmaKleen™ M-Aero at 160°F in an Agitating Immersion Washer for a minimum of 15-30 minutes